that purpose, and to increase the capacity and modify the texture of
the active material, we add a mineral additive in the cured plate
before formation with various percentages (1e15 %). The study was
based on X-ray diffraction analysis (XRD), thermogravimetry (TG),
differential scanning calorimetry (DSC) and scanning electronic
microscopy (SEM). The capacity of the different PAMs is determined
by galvanostatic discharge technique.