The chemically modified carbon paste electrodes were prepared
by thoroughly mixing graphite powder, paraffin oil and modifier
(Tu-SBA-15 in proportions of 5, 10, 15 and 20% (w/w), respectively.
The electrode body was fabricated from a glass tube of i.d. 5 mm and
a height of 3 cm