resulting in
high cellulose contents in substrate, which was facilitated for the
subsequent SSF operating at high cellulose content to obtain high
ethanol concentration. Because corncob was treated by alkali after
acid treatment, no furfural and HMF were detected by HPLC (data
not shown).