For T1 a linear increase for the MFR of both PP and PP_20%SP can be seen in Fig. 2, which results in a near doubling of the initial value after nine extrusions. This is coherent with the decrease of melt pressure monitored during sample production. Furthermore the incorporation of the scavenger in the material seems to have no additional effect on the MFR.