Drying process was carried out using a Christ lyophilizer (model 2-4α). Size and shape of nanoparticles were observed by transmission electron microscope (TEM, Philips-CM 120) operated at 100 keV. Morphology of nanoparticles was observed under a scanning electron microscope (SEM, Philips XL30) after gold film coating.