The same value of the
modulus and the tensile strength were observed at 5 wt%
of CNTs. While at 7 and 10 wt% the modulus was higher
than the tensile strength. At 1 wt% of CNTs the young
modulus increased by 25.95% compared to the pure SMR
CV60. At 3 wt% CNTs the increase in the young’s Modulus
was 141.92%.