Gradual uncovering of sub-surface material layers was performed
by electrolytic etching using a mixture
of 700 ml of phosphoric acid with 300 ml of distilled water and voltage between 1 and
1.6 V. Stress distribution on the tube wall thickness is given in Table 2.