As various parameters involved
in the process are mutually dependent on each
other, only the doping concentration was changed. The
doping concentration, i.e. aluminum/zinc atomic ratio as
a percentage (AI/Zn at.%), was varied from 0 to 4.5 at.%
in the solution.