To calculate travel speed, welding length was divided by the welding duration (cm/min). Direct current electrode negative (DCEN) was used preheating and inter pass temperature were 250C and 3000C, The chemical composition and mechanical properties of the base metal are listed in Tables 1 and 2, respectively.