The inhibited activity of the catalysts calcined
at 900 and 1000 C could be describable to the decrease of SBET to
0.2 m2 g1 due to the severe sintering of the catalyst particles as
observed by SEM (Fig. S1), though the formation of CaO phase
was completed.