ดีคาร์เบอร์ไรเซชัน is detrimental to
the wear life and fatigue life of
steel heat-treated components.
This article explores some factors that
cause ดีคาร์เบอร์ไรเซชัน while concentrating
on its measurement. In most production
tests, light microscopes are used to
scan the surface of a polished and etched
cross-section to find what appears to be
the greatest depth of total carbon loss
and the greatest
depth of combined FFD and partial
loss of carbon to determine the maximum
affected depth (MAD).