As listed in Table 3, the SGF group showed significantly lower hardness and higher values in springiness, cohesiveness, and
resilience than the WWN groups. However, there was a general trend of hardness increase as the MZ of WWF reduced from 125-mm to 72-mm; the hardness value of group 72-mm was significantly higher than of 125-mm group.