1) The three components (PP, PS, silica particles) and (PP, EVA, silica particles) were loaded to the mixing chamber simultaneously and compounded at 200°C for 5 min.
1) The three components (PP, PS, silica particles) and (PP, EVA, silica particles) were loaded to the mixingchamber simultaneously and compounded at 200°C for 5 min.