Apply KIWOSET HP using a soft brush onto both sides of the ready-made
and dried stencil. Allow the hardener to react a few minutes, then harden
either for approx. 60 min. at 35 - 40°C or at room temperature over night (at
least 20°C).
By deliberately selecting the hardening conditions, one can vary the
resistance of the screen. If the screen is hardened for example for 1 hour at
100°C, then the screen will be so resistant that it is no longer decoatable.
With fine meshes a fine haze of the hardener may remain in the open areas.
This haze is water and solvent soluble and disappears immediately after the
first few prints.
Notice: KIWOSET HP is not suitable for the hardening of chemically curable
photoemulsions.
DECOATING Screens hardened with KIWOSET HP can be decoated with PREGASOL