The 300 C-deposited film performed a higher electrical conductivity of 315 S/cm due to its higher chlorine doping level, larger grain size, and smoother film surface.
The 300 C-deposited filmperformed a higher electrical conductivity of 315 S/cm due to its higher chlorine doping level,larger grain size, and smoother film surface.