For obtaining the thermoplastic starch (TPS), starch granules were plasticized with glycerol in a weight ratio of starch/glycerol 70/30, as shown in Fig. 1, part I. The components were mixed at room temperature for 30 min. The obtained pulp was dried in an oven at 60 °C for 48 h.