A pure silver sheet with an area of 1.02.0 cm2 was used as the anode electrode ,ITO substrates (1.02.0cm2) with ZnO seed layer were used as the cathode ,and electrolyte solution was 0.003M/L zinc nitrate (Zn(NO3)2 6H2O) aqueous solution without any supporting electrolyte