Cattail was washed, dried, ground in a laboratory mill, and then impregnated with a 40 wt.% H3PO4 solution at a certain ratio. The resulting wet mass was placed in a muffle furnace and heated for several minutes with the final activated temperatures. It was cooled down afterwards to room temperature.