Especially, the one promoted with SiO2-TiO2 maximized both activity and methanol selectivity with 40.70% in CO2 conversion and 41.17% in methanol selectivity as compared to the one without promoter (15.81% in CO2 conversion and 23.31% in methanol selectivity).