Since both workability and compressive strength are of concern, a combination of 70% metakaolin and 30% blast furnace slag powders were mixed with the alkaline activating solution of W/B = 0.6, AE% = 18% and Ms = 0.75. The amounts of water, sodium hydroxide and sodium silicate