After steam explosion campaign, eight samples were selected for the following stages, in the range LogR0 4.2-
4.6; table 3 shows some pretreatment results, in terms of recovered WIS and recovered cellulose in the process.
Steam explosion efficiency, in percentage, is expressed as cellulose recovery; it defines recovered cellulose in WIS
compared to initial cellulose charged into the reactor.