The PVP@TBTsol was supplied at 1.0 ml/h by a springe pump. The electric field strength was set at 35 kV so as to keep a stable Taylor cone aerosolmode. The sprayed TiO2 spheres on the aluminum target were carefully collected and dried in air overnight in order to let the Ti precursors completely hydrolyzed.