Test parts produced in case study. Row 1: Top view of samples imaged using conventional microscope at 0.8 magnification. The malformed tabs on the printed RCP30 (post 1) sample are due to a combination of errors in the CAD file and damage during cleaning. Row 2: Large pocket imaged using conventional microscope at 6 magnification. Row 3: Surface roughness over 793 mm 881 mm area imaged using Alicona Infinite Focus at 10 magnification. Leveled, filtered, and plotted in SPIP. Shown with a 36 mm vertical range.