Fig. 14 depicts the creep compliance behavior of crosslinked
EOC samples at 150 C and 0.05 MPa stress level. As
we can see from the figure, elongation and thus creep reduces
as the peroxide content increases. Or, in other words
cross-linking and thus strength of the samples increases
when the peroxide level increases. This data are in good
agreement with earlier shown RPA results.