However we have recently determined that MW PS homopolymers (10e30 k) (not blends) appended with C13F27 end groups showed consistent decreases in Tg (~10e12 K) of the end functionalized PS relative to the isobaric PS homopolymer.
However we have recently determined that MW PS homopolymers (10e30 k) (not blends) appended with C13F27 end groupsshowed consistent decreases in Tg (~10e12 K) of the end functionalized PS relative to the isobaric PS homopolymer.