This enhanced crystallinity masked the effects of the BC/CNC fibre reinforcement in terms of single fibre mechanical properties. PLLA fibres filled with 2 wt.% C6-BC exhibited the highest yield strength of all fibres, 141 MPa, in comparisonto neat PLLA at 127 MPa (Table 2).