Effects of Strand Length
Specific mean values and coefficients of
variation of mechanical properties tested in tension,
compression and bending are given in Table 2.
The coefficients of variation, although seeming
relatively high (0% - 35%), are in the same range
of solid wood reported at 14% - 34% (Wood
Handbook, 1999).
For tension parallel to grain, the OSL made
of longer strands exhibited higher sUTS. Statistical
analysis showed that the results are highly
significant (Pr < 0.01). However, for the perpendicular
to grain direction there was no obvious
effect of the strand length on the sUTS. This is
explained by the very weak cohesive force (of
wood itself) in this direction. As a result, the sUTS
parallel to grain is about 35 times higher than that
of perpendicular to grain. The sTMOE parallel to
Effects of Strand LengthSpecific mean values and coefficients ofvariation of mechanical properties tested in tension,compression and bending are given in Table 2.The coefficients of variation, although seemingrelatively high (0% - 35%), are in the same rangeof solid wood reported at 14% - 34% (WoodHandbook, 1999).For tension parallel to grain, the OSL madeof longer strands exhibited higher sUTS. Statisticalanalysis showed that the results are highlysignificant (Pr < 0.01). However, for the perpendicularto grain direction there was no obviouseffect of the strand length on the sUTS. This isexplained by the very weak cohesive force (ofwood itself) in this direction. As a result, the sUTSparallel to grain is about 35 times higher than thatof perpendicular to grain. The sTMOE parallel to